AATCC 201 Textile Drying Rate Tester Hot Plate Method DR290F
AATCC 201 Textile Drying Rate Tester Hot Plate Method DR290F
【Scope of Application】
This tester is for functional moisture quick-drying fabric drying time and drying rate test (Hot Plate Method).
【Relevant standards】
etc.
The fabric drying rate analyzer determines the Moisture removal rate of textiles using the horizontal airflow method. It is used in the textile sector for quick drying to measure the Moisture evaporation rate of different types of fabrics.
The Textile Quick-Dry Tester simulates real-world drying. Its adjustable parameter system helps the operator create environmental conditions according to the test requirement.
A water-saturated fabric sample is placed in the fabric dehydration rate tester’s chamber. The focused fabric face direction is taken upward.
The hot air is passed over the specimen until it dries using the hot plate method. Test results are shown on the digital interface and can be printed.
Key Features
High Precision Sensors: The instrument is equipped with high-precision sensors which detect the slightest change in the evaporation process, dryness or weight loss.
Customizable Test Conditions: Apparatus simulates the real word-drying for atmospheric conditions. It has customizable test conditions which allow the operator to perform tests according to the different requirements.
Smart Test Analysis: The dry rate tester has software which shows the real-time data and gives shows a graph regarding the material’s drying behaviour.
Compact Design: The textile moisture evaporation tester has a compact design which is easily portable and takes less space which makes it suitable for lab and on-site use.
Learn More About All Our Dry Rate Testers!
ASK FOR A QUOTE
We will contact you in one working day. Please pay attention to the email with suffix @darongtester.com
Related products
- Fabric Testing Instrument
ASTM D3787/ASTM D6797 Textile Bursting Strength Tester YG(B)031S
Rated 0 out of 5