ASTM D4970/ISO 12945 2 Martindale Pilling & Abrasion Tester YG(B)401T
ASTM D4970/ISO 12945 2 Martindale Pilling & Abrasion Tester YG(B)401T
【Scope of Application】
This tester is used in textiles, membrane materials resistant to wear and abrasion, and the appearance change (Pilling) performance test (Martindale method).
【Relevant Standards】
GB/T21196(China national standard drafting enterprise)
FZ/T98014 (Main drafting enterprise )
GB/T 4802.2
FZ/T 20020
ASTM D4966
JIS L1096
ASTM D4970
GB/T13775
ISO 12945 2
ISO 12947
IWSTM196 / TM112
M&S
etc.
Abrasion and Pilling are the most common fabric problems faced by end users. They are caused by pill or beads forming and degrading. These problems are mostly seen in used garments. Before manufacturing garments, fabrics are tested for their change in appearance and performance. This helps the manufacturer meet the required resistance for garments.
The YG(B) 401T Martindale Abrasion Tester measures fabric wear and tear and appearance change. Separate methods and different machine settings are used for pilling and abrasion. Fabric is evaluated by change of appearance and difference in weight.
Key Features
Multiple working Stations: This pilling tester can test up to 09 fabric samples at one time, which saves time.
Multi-direction Movement: The Lissajous movement of the device makes it more effective and real than testers with linear movement.
Adjustable Speed Movement: The speed of the abrasion tester can be adjusted between 20 to 70 RPM.
Abundant Counting Range: Users can extend their counting range up to 999999 movements.
2 Grinding Blocks: For pilling and abrasion testing, 198g and 155g friction heads are used.
Global Compliance: This pilling and abrasion machine can be used worldwide as it complies with ISO, GB, FZ, TM, M&S and JIS industrial standards.
User-Friendly Interface: The 7-inch touch-screen has multiple languages, which makes it easier to input commands for performing tests.
Learn More About Our Martindale Pilling and Abrasion Testers!
Related Resources
Practical Explanation on ISO 12947 Abrasion Resistance Test by Martindale Method
ASK FOR A QUOTE
We will contact you in one working day. Please pay attention to the email with suffix @darongtester.com
Related products
- Fabric Testing Instrument
ASTM D4964 Elastic Comprehensive Strength Testing Machine Y(B)091L
Rated 0 out of 5