Light Fastness Tester YG(B)611TC3
Light Fastness Tester YG(B)611TC3
(National Patent ZL201520754700.X)
[Scope of application]
It is used for light fastness and weather fastness test in dyeing fastness test. It can also be used for light fastness test and light aging test of paint, pigment, coating, rubber, plastic, wood floor and paper and other materials.
[Related standards]
GB/T8427 (China national standard drafting company)
GT/35256 (China national standard drafting company )
GB/T15102-2006
GB/T14576
GB/T15104-2006
GB/T8430
AATCC TM16
ISO105-B04
ISO105-B02
ISO 4892-2
【 Instrument characteristics 】
Internet of Things + solutions
1, support Ethernet wired network, Wifi and Bluetooth data interaction;
2, support wechat mini program and Web device monitoring and alarm;
3, support monitoring and management of multiple devices at the same time;
4, support the storage and analysis of large capacity test data;
5, support each station independent output test data;
6, support the test report form output, and can attach the sample before and after the test picture information;
7, support device software OTA growth.
Innovative characteristics
1, light intensity digital setting, real-time monitoring, automatic adjustment, in order to meet the stability requirements of different standards for the test light source (can be switched 420nm; 300-800nm or 300-400nm band monitoring);
2, standard blackboard thermometer (BST), blackboard thermometer (BPT) can be selected to use, and the same station (equidistant) with the sample detection, truly reflect the test condition of the sample;
3, the measured data after CPU processing in numbers, charts, curves and other ways displayed on the color screen, without stopping observation;
4, microchip 32-bit intelligent CPU, efficient real-time control, to ensure the same test environment accurate reproduction;
5, 10.4 “color industrial computer display control, a variety of test monitoring mode (digital, chart), easy to control, intuitive and clear.
6, All sample clips can be timed separately, and different samples can be tested on the same machine, which is convenient for testing and monitoring and reduces operating costs;
7, rated 1300W long arc xenon lamp technology, high efficiency and energy saving, real simulation of daylight spectrum;
8, industrial temperature control (refrigeration) system, the temperature adjustment in the test chamber is rapid and stable;
9, built-in self-circulation system and air filtration system, greatly reducing environmental requirements;
10, European traceable spectrum analyzer, multiple measurement calibration;
11, a test can run for 1000 hours of quality assurance.
12, built-in multiple sets of standard experimental procedures, and up to 20 customizable experimental procedures can be named;
13, support irradiance meter, blackboard (black label) thermometer, temperature and humidity sensor convenient calibration mode;
14, with the instrument life running record, lamp running status monitoring and prompt;
【 Technical parameters 】
- Temperature control range of test chamber: (20 ~ 50)℃; Accuracy: ±2℃
- Humidity control range of test chamber: (15 ~ 95) % RH, accuracy: ± 5%RH
- Test time control range: 0 ~ 999:59 (h: min); Accuracy: ±1min
- Effective control range and control accuracy of irradiance:
(0.80 ~ 1.50)W/m2/420nm accuracy: ±0.02W/m2
(30-50)W/m2/300-400nm Accuracy: ±2W/m2
(350-600)W/m2/300-800nm Accuracy: ±10W/m2
Digital setting, automatic compensation
- Xenon lamp source:
- Xenon arc lamp rated power: 1.3kW;
- Color temperature: 5500K ~ 6500K;
- Sample:
- sample rack rotation speed: 5rpm; Accuracy: ±3 seconds
- Sample clip distribution diameter: 286mm
- Size and number of specimen holder:
| GB/ISO | AATCC (Optional ) | |
| Specimen holder size | 208mm×48mm | 208mm×92mm |
| Maximum sample size | 122mm×45mm | 122mm×90mm |
| Maximum exposure area | 110mm×33mm | 110mm×50mm |
| Maximum number of packages | 13 PCS | 6PCS |
- Each sample holder is timed separately: range: 0min ~ 999:59 (h: min); Accuracy: ±1min
- Sample thickness: ≤8mm
- Standard Black Label thermometer (BST) range:
(30 ~ 75)℃; Resolution :0.1℃, accuracy: ±2℃
Or optional Blackboard Temperature (BPT) range:
(30 ~ 70)℃, resolution :0.1℃, accuracy :±2℃
- Power supply: AC220V±10% 50Hz 5.5kW
- Overall dimensions: 1130mm×760mm×1895mm
- Weight: about 380kg
Learn More About All Our Light Colorfastness Testers!
Related Resources
Insights to Textile Colorfastness Standards from A Front-Line Technician
An Overview to Lightfastness Test for Textile
A Guide to ColorFastness in Textile Dyeing: What You Need to Know for Long-Lasting Vibrance
ASK FOR A QUOTE
We will contact you in one working day. Please pay attention to the email with suffix @darongtester.com
Related products
- Fabric Testing Instrument
ASTM D3787/ASTM D6797 Textile Bursting Strength Tester YG(B)031S
Rated 0 out of 5