ASTM D1777/ISO 9073 Thickness Tester YG(B)141G
ASTM D1777/ISO 9073 Thickness Tester YG(B)141G
【Scope of application】
This tester is used for measuring the thickness of various fabrics and thin materials.
【Related standards】
GB/T3820
GB/T24218.2(general class)
FZ/T01003
ASTM D1777 (customization)
ISO 5084-1996
ISO 9073
etc.
The material thickness gauge measures the thickness of fabrics, textiles, and other thin materials. A precision gauge determines the thickness of fabric samples in a laboratory.
In this equipment, the fabric whose thickness is to be determined is kept on the flat anvil, and a circular pressure foot is pressed on it from the top under a fixed load.
The dial indicator directly gives the thickness in mm. The principle of measurement of fabric thickness is based on the precision measurement of the distance between two parallel plates separated by the cloth when a known pressure is applied and maintained on the plates.
The fabric thickness meter is essential in textile industries to ensure the required thickness of fabrics for consistent results.
Key Features
Compliance: The textile thickness meter follows the guidelines and meets the compliance of international standards ASTM D1777/ISO 9073(customization).
Adjustable Pressure: The cloth thickness measuring device has the option of adjustable pressure, which helps to set the pressure according to the thickness of different fabric types.
Stable Anvil: The material thickness tester has a stable anvil, which helps to give consistent results without the risk of variation on repeated trials.
Pressure Foot: This cloth thickness measuring device utilizes a pressure foot that applies a controlled uniform force to ensure equal compression on the specimen.
Wide Application: The material thickness tester is suitable for wide applications on various materials, including textile composite and other compressible thin materials.
Durable Construction: The thickness tester is built with high-grade quality material, which ensures long-term use and durability.
Compact and Portable: The fabric thickness measurement instrument has a compact design, making it suitable for use in the laboratory and production site.
Learn More About Our Fabric Thickness Testers!
Related Resource
ASK FOR A QUOTE
We will contact you in one working day. Please pay attention to the email with suffix @darongtester.com
Related products
- Fabric Testing Instrument
ASTM D4964 Elastic Comprehensive Strength Testing Machine Y(B)091L
Rated 0 out of 5