How to Conduct AATCC 16.3 Light Colorfastness Test

DR4000 is a Water-Cooled Type Xenon Arc Chamber to test the material’s colorfastness to light. In this article, we’ll demonstrate the DR4000 Xenon Arc Weathering Tester. This test is conducted according to AATCC 16.3 standard.

AATCC 16.3 Light Colorfastness Test

Sample Preparation:
Cut a specimen ensuring the exposed area is at least 30 x 30 mm.

Mounting the Specimen:
Place the test side of the fabric facing upward, secure both sides on the specimen holder. Repeat this process for the remaining specimens using the same method.

Open the test chamber door, place the specimens inside the instrument, then close the door.

Instrument Setup:
Turn on the pure water system.
Click “Standard Settings”, use the up/down keys to select the appropriate test standard.
Click “Query” to view the test parameters, then click “Return”.
Once the standard is selected, go to “Run Time”.

Set an appropriate exposure time based on the standard and customer requirements.
Confirm → Confirm → Return.

Click “Start” and wait for the xenon lamp countdown to complete.

Once the countdown finishes, the xenon lamp turns on and the rotating rack starts—test begins.

Upon test completion, the instrument shuts off automatically.
After the xenon lamp cools down, remove the specimen and proceed to grade (evaluation).

This experiment follows AATCC 16-3

Click to learn about the procedure of ASTM, ISO, GB, etc.

Click to learn about Xenon Arc Test Chamber

Related Resources

Mastering Color Fastness: Test Methods and Techniques for Exceptional Results

Air-Cooled and Water-Cooled? Choosing the Right Light Fastness Tester for Your Lab

    Scroll to Top

    ASK FOR A QUOTE

    We will contact you in one working day. Please pay attention to the email with suffix @darongtester.com