The maximum load a yarn or fabric can withstand before breaking is its tensile strength. There are three types of tensile testing methods: CRL (Constant Rate of Loading), CRE (Constant Rate of Extension), and CRT (Constant Rate of Traverse). Let’s know more about the CRE Tensile Test, and look at the relationship and differences among them in this article.
What is the CRE Tensile Tester?

Definition & Function of A CRE Tensile Tester
The CRE tensile tester, which is also known as the Constant Rate of Extension tester, is used to measure the fabric strength, elongation, and elasticity and to determine the maximum tensile force that the fabric can withstand before its breaking point. For this purpose, the specimen is pulled at a constant rate of extension until it breaks.
Function
DaRong’s Electronic Strength Machine YG(B)026HC model works on the CRE principle. It applies a uniform crosshead tensile force to the specimen, resulting in stable stress-strain rates and giving reliable results.
This tester has the speed limit from 0.01 to 1000 mm/min, and can be adjusted easily to determine the peak load and elongation data.
This Electronic tensile tester is equipped with a microcomputer that records the precise force measurement and deformation values of materials such as textiles, rubber, plastic, and composites.
Role of Constant Rate of Extension in Testing
In the Constant Rate of Extension (CRE) method, we apply a constant rate of tensile force to the fabric specimen, which produces a stress-strain curve generated by the tester’s microcomputer.
Tester’s software generates the stress-strain graph by precisely measuring the applied tensile force and elongation. Darong’s CRE-based testers, such as Electronic Strength Machine YG(B)026HC, and Chemical Fiber Filament Strength Tester YG(B)021HL, rely on servo-driven cross heads, which ensure the stable stretching control.
For example, the YG(B)021HL also has the speed range from 10–1000 mm/min, which is ideal for fibre and filament testing. In CRE testing, we maintain a fixed crosshead speed, such as 50 – 300 mm/min, which helps to avoid the force variation during the test.
CRE testing eliminates the risk of overshoot that leads to premature microfracture and minimises the dynamic loading errors.
CRE vs CRT vs CRL — Key Drive/Control Modes Explained
How CRE Differs from CRT (Constant Rate of Traverse)
The Constant Rate of Extension or Elongation (CRE) tensile tester has one fixed clamp, in which one end of the yarn, leaf or fabric specimen is clamped, and the other clamp is moveable, which is screw driven. It pulls the specimen downward while maintaining a constant rate of elongation.
The Constant Rate of Traverse (CRT) tensile tester has movable top and bottom clamps. The top clamp moves upward through the pulley. The bottom clamp moves downward through a screw-driven mechanism.
In this way, the fabric CRT tensile tester applies force to both ends of the specimen until the specimen breaks. The main difference between them is that the CRE testing method has controlled stretching, which gives more reliable results due to a constant rate of elongation.
While in CRT, we can control the clamp’s speed, but the movement of both jaws can cause variable force, which may lead to less reliable results. That’s why modern labs prefer the CRE tensile tester.
How CRE Differs from CRL (Constant Rate of Loading)
In Constant Rate of Loading (CRL) tensile testing, we fix the one end of the fabric specimen in a fixed clamp. This clamp is not movable and is placed at the upper end. The second end of the fabric or yarn will be hanging freely downward.
To determine the tensile strength through the CRL method, we will apply the load on the free end, and the load will be increased at a constant rate until the fabric breaks. The load at which the specimen breaks is called the tensile load of the specimen and indicates the fabric’s tensile strength.
In CRL, one jaw is fixed, usually at the upper end, and the second jaw is movable, applying the load at a constant rate to measure the fabric’s breaking point. You can test single yarn, lea, or woven fabric through this testing method.
The main difference between CRL and CRE is the load application. The CRL applies load gradually increasing up to the breaking point, while in CRE the load is applied slowly through the screw-driven by maintaining the constant rate of elongation.
Why CRE Technology Is the Modern Industry Standard?

The constant rate of Extension (CRE) tensile testing method provides more accurate results by maintaining a fixed extension rate, which minimises the risk of stress-strain rate variation.
Modern CRE tensile tester, such as Darong’s YG(B)026HC model, uses high-precision guide rolls, which avoid the risk of slippage and give accurate results within ±1% accuracy.
As in the CRE tensile tester, one jaw is fixed, whereas in the CRT tensile tester, the stress-strain behaviour remains constant with little variation.
CRE tensile testing method meets the requirements of ASTM D5034/D5035, ISO 13934-1, and ISO 2062. The tensile strength of textiles, plastics, rubber, and composites can be tested using the CRE tensile tester.
Technical Features Professional Buyers Should Evaluate
Load Cells, Grips, Sensors, and Crosshead Performance
Darong’s CRE tensile tester YG(B)026HC has a high-precision load cell, which has the range of up to 10K N, and gives resolutions from 5N to 100N, depending on the range. Pneumatic grips help to avoid the slippage under high tension.
CRE tensile tester by Darong is equipped with guide rolls and a reinforced cross-head that help to maintain uniform motion under high load.
Software Control, Data Acquisition, and Test Curve Analysis
The tester has a digital interface supporting a 2000 Hz data sampling rate and real-time DSP processing for stress-strain curves.
The speed of screw-driven jaw can be adjusted according to test requirement for getting reliable and accurate results. CRE tensile tester gives test results within the + 1% accuracy.
Conclusion
CRE tensile testing works on the principle of Constant rate of Elongation, which provides stress–strain rate results with an accuracy of ±1. If we see as compare to CRT and CRL, the CRE gives more stable results due to screw – driven load application and having one fixed clamp.
This setting minimizes the force variation and dynamic loading errors, manual grips hold the specimen firmly to avoid the specimen’s slippage under tention. These are the reasons modern labs prefer the CRE tensile testing method compared to CRT and CRL.
FAQs
What is a CRE tensile tester?
A CRE tensile tester pulls the specimen at a constant extension rate to measure tensile strength, elongation, and breaking force.
Why is CRE testing more accurate than CRT or CRL?
Because CRE testing maintains a fixed crosshead speed, which avoids force variation and yields highly stable stress-strain results.
What materials can be tested with a CRE tensile tester?
Textiles, yarns, fibers, plastics, rubber, and composites can be tested through CRE method.
Related Resources
How to Perform ASTM D4964 Cyclic Stretch and Recovery Test Using a Tensile Tester
ISO 2062: Guide to Yarn Tensile Testing
Difference between Tear Strength and Tensile Strength
Fabric Tensile Tester – An Ultimate Guide for Textile Manufacturers and Laboratories