ASTM D6695 Xenon Arc Light Fastness Testing
The ASTM D6695 standard measures the effectiveness of various painted and coated materials under controlled environmental conditions. Accurate Xenon Arc light fastness results mainly depend on control of irradiance, Stable BST, adherence to human testing regulations, correct sample preparation, and regular calibration of the testing chamber. Major Measurements of Xenon Arc Light Fastness Testing How Does Xenon Arc