The fabric’s tear strength is essential when testing fabrics’ durability and mechanical qualities. In this article, you will learn about tear strength, its importance, and how to test a fabric using ASTM D2261. After reading this article, you will understand its purpose and its necessity for fabrics.

What is Fabric Tear Strength?

The force needed to tear a fabric is known as its tear strength, an important aspect that determines a fabric’s capacity to withstand damage with time. The ASTM has developed a standard test procedure for evaluating fabric tear strength. This global standard assures standardization and accuracy in the measurement process. This test method uses a computer-based constant-rate-of-extension-type (CRE) tensile testing machine to test the tearing strength of fabrics using the tongue tear process.

An Introduction to ASTM D2261

A common name for ASTM D2261 is the “Tongue Tear Test.” It also has the name of Trapezoid Tear Test.  The cloth specimen used in this test resembles a tongue or trapezoid originating from the term.

ASTM D2261 uses a tensile testing machine with a Constant rate of Extension type. A rectangular specimen with a cut in the middle of a shorter side creates a two-tongued (trouser-shaped) specimen with one tongue clamped in the upper jaw and the other in the lower jaw. The force is then applied to spread the tear by gradually increasing the gap between the jaws. The force which is applied to the fabric is also recorded. A data recording-based computer evaluates the force needed to continue the tear.

Woven fabrics are typically more robust and have more tear resistance than non-woven fabrics. This is because woven fabrics are strengthened by the intersecting lines of threads, which collectively form a robust barrier. Longer floats in woven fabrics make it easier for threads to slide and cause fabric distortion, which causes more yarns to share the load. Woven fabrics typically have higher tearing strengths. For example, twill and sateen weave fabrics have a comparatively higher tearing strength than plain ones. Although a nonwoven fabric can have more tear strength than woven fabric it depends entirely on the materials used to make it.

Similar Standards to ASTM 2261

  1. ISO 13937 = In this method, a single tear technique is used to assess fabric tear force.
  2. GB/T3917 = The ballistic pendulum (Elmendorf) method for determining the tear force of textile textiles is described in GB/T 3917.
  3. BS 4303 = It describes a wing rip tear test method.

Picking the appropriate standard depends on the type of fabric, its particular use, and the qualities that need to be measured. Each standard has unique sample criteria and test procedures.

Testing Procedure of ASTM D2261

Apparatus

CRE Type Machine
CRE Type Machine
  • CRE-type Tensile Testing Machine, preferably with a computerized interface. (Figure 1)
  • Clamps (25 x 75mm)
  • Cutting Die or Template as shown in Figure 1.

Sample Preparation & Conditioning

  • Cut rectangular specimens having dimensions 75 x 200 mm ±1
  • Consider the shorter length as the test direction.
  • Make a preliminary cut having 75 mm ± 1 mm length at the center of the sample width.
Sample Cutting Dimensions in mm
Sample Cutting Dimensions in mm
  • Take five specimens along the length and five specimens along the width of the fabric.
  • Test the specimens in the standard atmosphere for testing textiles, which is 21 ± 1°C (70 ± 2°F) and 65 ± 2 % relative humidity.
  • At the beginning of the test, set the spacing between the clamps at 75 mm ± 1 mm.
  • Set the testing speed 50 ± 2 mm/min.

ASTM D2261 Testing Procedure

  1. Place the specimen into the testing machine clamps. For the tearing force to be exerted correctly, the narrow top edge must align with the clamps.
  2. Keep in mind that the cloth is correctly oriented and has no slack.
  3. Once the machine is running, a force will be applied to the sample. The device will calculate the force needed to start and spread the tear.
  4. Record the force necessary to continue the tear. It is generally expressed in pounds-force (lbf) or Newton (N).
  5. Repeat the process for all specimens.
  6. Note the maximum tear force of each sample and then calculate the average.

Textile Lab Report Formation

  1. Describe details about the specimen’s material. (e.g., yarn count and material, Type of Weave, Type of finish if applied, etc.)
  2. State the kind of testing apparatus and if modified clamps are used.
  3. Mention the speed of the machine while testing.
  4. State that this test is by ASTM D2261.

Experiences and insights on ASTM D2261 Tongue Tear Test

  • Ensure that when you cut the sample, the threads traveling in the long direction are parallel to the length. This way, when the slit is cut, the rip will occur between the yarns rather than across them.
  • Don’t take specimens nearer to one-tenth of selvage.
  • Materials with stretch properties must relax for 24 hrs before preparing a sample.
  • Verify that the testing machine has appropriately aligned grips or clamps and is calibrated.

Conclusion

The Tongue Tear Test (ASTM D2261) is an essential technique for evaluating the tearing strength of textiles and offers insightful data regarding their resilience to tearing across a range of industries. This standard assists in acquiring of accurate and consistent measurements for various fabrics by manufacturers, designers, and quality control specialists by offering recommendations for carrying out tear strength tests and computing tear strength values. Companies can fulfill customer demands, legal regulations, and quality control standards by following the ASTM standard. This will eventually result in better products and satisfied consumers.

FAQs

  1. Which fabric has high tearing strength?

Usually, those fabrics that have long float weaves show higher tear strength.

  1. How can we improve the tear strength of the fabric?

It depends on the appropriate fiber type, tighter weave or knit, and addition of reinforced components. Special finishes or coatings over the fabric also enhance its tear strength.

  1. Can we use the Tongue Tear Test for all types of fabrics?

Most textile fabrics, woven, knitted, or unwoven, can be tested using this procedure. Extremely lightweight or high-strength fabrics like Kevlar should not be tested with them as they require specialized equipment for handling.

  1. What is the unit of tear strength?

The unit can be in SI units. Mostly, an inch-pound is used as a standard.

Related Resources

Fabric Tensile Tester – An Ultimate Guide for Textile Manufacturers and Laboratories

ASTM D5034/ASTM D5035 Electronic Strength Machine YG(B)026HC

What is fabric strength and how to test

    Scroll to Top

    ASK FOR A QUOTE

    We will contact you in one working day. Please pay attention to the email with suffix @darongtester.com