AATCC 117/AATCC 133 Color Fastness to Scorch and Sublimation

The AATCC 117 test standard evaluates the colorfastness of fabric to dry heat. In this test procedure, dry heat is applied without pressing the specimen. The AATCC 133 test standard measures a fabric’s colorfastness when subjected to intensive heat with pressing.

Colorfastness in Textile 

Colorfastness in Textile

Colorfastness (CF) means how well a fabric keeps its colour without fading or bleeding when washed, exposed to light, rubbed, scorched, dry heat or sweat. It’s essential for clothes and fabrics because it ensures the colours stay bright and don’t change over time.

Colourfastness properties are the main parameter in the textile market, used to sell products and ensure customer satisfaction. Two main organizations, ISO and AATCC, provide guidance for standard testing procedures to determine fabric CF properties.

Factors affecting Colorfastness 

What makes some fabrics keep their colour well while others can ruin a whole load of laundry? CF depends on the following things.

  1. Type of Fibre 

Different fibers have different qualities. For example, polyester usually holds colour better than nylon.

  1. Dye Fastness and Application 

The colour itself also plays a role. Darker colours tend to fade more quickly than lighter ones. The dye used, and its application to the fabric can affect how long the colour lasts. Some dyes stick better to certain fabrics than others.

  1. Fabric Properties

The fabric’s properties are also important. Some materials naturally hold dye better. Also, if the fabric has been treated before dying, like with special chemicals, it can change how well the colour stays.

  1. Fabric Condition 

Damage to the fabric or any added finishes can also affect the colour. For example, if the fabric’s surface is worn out, the colour might also not last.

  1. Dyeing Process

Finally, the dyeing process itself matters. If the fabric is washed (a step called “soaping”) after dyeing, it can help set the colour.

  1. Finishing

How the fabric is finished and treated after dyeing also affects colorfastness properties. These factors determine whether a fabric will keep its colour or bleed in the wash.

What is the Difference in Scorching and Sublimation? 

Scorching        

Scorching is damage when fabric or other materials are exposed to high heat. This can cause the fabric to change colour, get charred, or even burn. For example, an iron that is too hot can scorch the fabric, leaving marks or discoloration.

In textile testing, there is something called a scorch test. This test checks how well a fabric can handle heat without getting damaged or changing colour. It helps to see if the fabric can look good even when pressed with a hot iron or exposed to dry heat.

Scorch tests are essential because they show how colorfast a fabric is under heat. This helps manufacturers and users understand whether the fabric will hold well during ironing or other heat-related processes.

Sublimation

Sublimation is a process where material transforms from a solid state to a gaseous state without converting into a liquid. A typical example is dry ice, which is solid carbon dioxide. Dry ice turns straight into a gas at room temperature, skipping the liquid stage.

In heat transfer printing, sublimation is used to print designs on materials like polyester. Special sublimation ink is heated; instead of turning into a liquid, it turns into a gas. This gas bonds with the fabric’s fibers, creating a colorful and durable image.

In textile testing, sublimation tests are used to check how well the fabric’s colour holds up under heat under pressing and whether the fabric stays the same size and shape when exposed to heat. These tests help ensure the fabric can handle heat without losing colour or getting damaged.

AATCC 117/AATCC 133 Test Method 

Colour Fastness Tester performs the testing standard of AATCC 117/AATCC 133 to Scorch and Sublimation. We will conduct this test on the YG (B) 605G tester built by Darong.

AATCC 117/AATCC 133 Color Fastness Testers to Scorch and Sublimation YG (B) 605G

Turn on the power switch, set the parameter, and then set the test temperature according to the standard.

Set up Parameter

The upper temperature is 150 degrees Celsius, and the lower temperature is 150 degrees Celsius. Set the timer for 30 seconds.

Set Time and Temperature

After setting the time and temperature, press the return key. Enter the test interface. Lift the upper heating block. Click sublimate to heat.

Click sublimate to heat

Take a sample size of 40 by 100 millimeters. Take the exact size of the multi-fibre fabric. Sew the short edge of the multi-fibre fabric and sample.

Take a sample size of 40 by 100 millimeters

Wait for the instrument to warm to the set temperature before starting the experiment. Then, place the combined sample flat on the heating block.

Place the combined sample flat on the heating block

Lower the upper heating block and start the timer. Remove the sample when the timer is over. The sample was placed in a standard atmosphere for four hours.

Place the sample in a standard atmosphere for four hours

The staining and shade change are rated with the grey scale or standard.

Conclusion 

The AATCC 117 test standard evaluates the colorfastness of fabric to dry heat. In this test procedure, dry heat is applied without pressing the specimen. The AATCC 133 test standard measures a fabric’s colorfastness when subjected to intensive heat with pressing.

FAQs

What is AATCC 117?

The AATCC 117 test standard evaluates the colorfastness of fabric to dry heat. In this test procedure, dry heat is applied without pressing the specimen.

What is AATCC 133?

The AATCC 133 test standard measures a fabric’s colorfastness when subjected to intensive heat with pressing.

Why is colorfastness important in textiles?

Colorfastness properties are the main parameters in the textile market, and they are used to sell products and ensure customer satisfaction.

What is the Difference in Scorching and Sublimation?

Scorching is damage when fabric or other materials are exposed to high heat, and sublimation tests are used to check how well the fabric’s colour holds up heat under pressing.

What is the time and temperature for AATCC 117/AATCC 133 test?

The temperature is set at 150 Celsius, and the time is set for 30 seconds.

 

Related Resource

AATCC 117/AATCC 133 Color Fastness Tester to Scorch and Sublimation YG(B)605-3

AATCC 117/AATCC 133 Scorch Tester/Sublimation Fastness Tester YG(B)605DC

Mastering Color Fastness: Test Methods and Techniques for Exceptional Results

    Scroll to Top

    ASK FOR A QUOTE

    We will contact you in one working day. Please pay attention to the email with suffix @darongtester.com